J. Eng. Gas Turbines Power. September 2011, 133(9): 091301.
Published Online: April 14, 2011
... loading conditions, nanoindentation was used to study the mechanical properties (Young’s modulus and hardness) of the components in the TBC system and their evolution with temperature and time. The effect of uniaxial in-plane compressive creep strain on the rate of growth of the thermally grown oxide...